A. Schulman, Inc. POLYBATCH™ Poly Off-White P90062PF, Concentrate Based In Polypropylene
Subcategory: Polypropylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: Description POLYBATCH® P90062PF is an off-white color concentrate based in polypropylene. This concentrate was designed to provide color polypropylene film, extrusion, and molding applications. POLYBATCH® P90062PF is typically recommended for use at 30% addition levels.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Ash
- Moisture (max)
- Pellet Count
|
|
|
|