A. Schulman, Inc. POLYBATCH™ Popular Choice White HS80660, Concentrate Based In Polystyrene
Subcategory: Polystyrene; Additive/Filler for Polymer; Thermoplastic
Material Notes: Description POLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive letdown mixing. POLYBATCH® HS80660 is typically recommended for use in extrusion film and sheet, thermoforming, and injection molding applications.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Ash
- Moisture (max)
|
|
|
|
| Property Data |