A. Schulman, Inc. POLYBATCH™ U-0294-L Blowing Agent, Concentrate Based In PE
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: Description POLYBATCH® U-0294-L is 20% active endothermic blowing agent concentrate based in PE. This concentrate is white in color, non-tinting and is designed for use in PE, and PP applications to reduce part density and eliminate sink marks with very little surface splay. POLYBATCH® U-0294-L produces optimum blow at 380°F and is typically used at 2 to 10% addition levels depending upon customer specific applications requirements.
Information provided by A. Schulman.
| Available Properties |
- Additive Loading
- Pellet Count
|
|
|
|
| Property Data |