A. Schulman, Inc. POLYBATCH™ White LL8425 AP, Concentrate Based In LLDPE
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LLDPE
Material Notes: Description POLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phenolic yellowing/pinking, while optimizing whiteness and thermal stability. POLYBATCH® LL8425 AP also provides optimal dispersion and opacity with excellent letdown mixing. POLYBATCH® LL8425 AP is recommended for use in extrusion film and sheet as well as injection molding applications.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Ash
- Moisture (max)
- Pellet Count
|
|
|
|
| Property Data |