A. Schulman, Inc. POLYBATCH™ White P8555 T2, Concentrate Based In Homopolymer Polypropylene
Subcategory: Polypropylene; Additive/Filler for Polymer; Thermoplastic
Material Notes: Description POLYBATCH® P8555 T2 is a premium white masterbatch containing 50% TiO2 based in homopolymer polypropylene. This product is processed through 300x300 mesh screens and offers premium dispersion POLYBATCH® P8555 T2 is recommended for use in cast, blown, OPP, or BOPP film applications requiring high loading levels with premium dispersion.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Melt Flow
- Ash
- Moisture (max)
- Pellet Count
|
|
|
|
| Property Data |