A. Schulman, Inc. POLYBATCH™ XU-2013-LD, Concentrate Based In LDPE
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LDPE
Material Notes: Description POLYBATCH® XU-2013-LD is a 10% active, exothermic blowing agent masterbatch based in LDPE. This masterbatch is orange/yellow in color and can be used in polyethylene, polypropylene, and polystyrene applications.