A. Schulman, Inc. POLYBLAK™ Polyblak 3422, Black Color Concentrate, 35% Carbon Black Based In LDPE
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LDPE
Material Notes: Description POLYBLAK® Black 3422 is a black color concentrate containing 35% carbon black based in LDPE. This masterbatch is designed to provide excellent UV absorption with a regular brown undertone and pigment particle size of 19 nanometers. POLYBLAK® Black 3422 is specially formulated for use in automotive polypropylene and compounding and injection molding applications. POLYBLAK® Black 3422 is typically recommended for use at 5% addition levels.
Information provided by A. Schulman.
| Available Properties |
- Specific Gravity
- Carbon Black Loading
- Moisture (max)
|
|
|
|