Arkema Altuglas® 84 L Acrylic-Styrene Copolymer
Subcategory: Polystyrene; Acrylic; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Material Notes: ALTUGLAS 84 L is a new type of acrylic polymer produced by ATOHAAS which increases the range of material for injection molding applications. ALTUGLAS 84 L is a styrene methylmethacrylate copolymer studied in order to meet the need for an high performance clear product able to resist in applications requiring good crazing resistance. Outstanding features: - clarity and brilliance
- scratch resistance
- easy processing
- UV stability
- resistance to household detergent and dishwasher cycling
- good crazing resistance
Typical application :
- salad bowls, tumblers, cutlery handles and other house ware parts that require resistance to dishwasher cycling.
- medical devises.
- bath room accessories.
ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|