Arkema Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon, Aromatic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyamide
Material Notes: Designation ISO 1874-PA12/xx,MHLR,12-020 Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion. Transparency even thick. High resistance to environmental stress cracking. Good mechanical properties. Good thermal resistance. Dimensional stability. Example applications: Glasses. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|