Arkema Evatane® 1003 VL 4C Ethylene Vinyl Acetate
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: EVAC
Material Notes: EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |