Arkema Kynar® 710 PVDF
Subcategory: Fluoropolymer; Thermoplastic; PVDF
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinylidenefluoride
Material Notes: Designation ISO 12086-PVDF-E,M1G1N,P.?E4.I.C.F.C,, ?(20-35) Kynar PVDF are fluorinated thermoplastic homopolymers. Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermomechanical properties. Main applications of Kynar: corrosion protection in the chemical industry, coating (painting, coextrusion), off shore, wire and cable. Kynar 710 is a grade of granules for injection molding, rotomolding applications and multifilament extrusion. This product is ANSI/NSF Standard 61 certified. Powder form available as Kynar 711. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|