Arkema Kynar® FLEX 2801 PVDF
Subcategory: Fluoropolymer; Thermoplastic; PVDF
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinylidenefluoride
Material Notes: Designation ISO 12086-VDF/HFP-K, EDN, N. ?E7.D.G.B.C,, ? (3.5-7.5) Kynar FLEX PVDF are fluorinated thermoplastic copolymers. Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness to UV, high barrier properties, high purity, good mechanical and thermomechanical properties. Main applications of Kynar FLEX: corrosion protection in the chemical industry, coating (painting, coextrusion), off shore, wire and cable. Kynar FLEX 2801 is the powder form of the Kynar FLEX 2800. To be used as an additive in LLDPE to improve the extrusion rate. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Dielectric Constant
- Dissipation Factor
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|