Arkema Lacovyl® EF 701 PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinyl Chloride; Polyvinylchloride
Material Notes: LACOVYL EF 701 is a vinyl chloride homopolymer manufactured by emulsion polymerization process for the preparation of plastisols. * MAIN CHARACTERISTICS Viscosity index (ISO 1628-2):125 ml/g,(K value:70). * APPLICATIONS LACOVYL EF 701 may be used in the following areas: - compact layer: wall coverings or coated fabrics.
- foam layer by mechanical or chemical techniques.
- rotational molding: toys, bumpers,buoys, car parts.
- dip molding.
- slush molding.
- cap closures.
ISO data provided by the manufacturer, Arkema.
|
|
|