Arkema Lacovyl® GB 1150 M PVC, Pipe Grade
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinyl Chloride; Polyvinylchloride
Material Notes: LACOVYL GB 1150 M is a vinyl chloride homopolymer produced by the Elf Atochem's mass polymerization process. Its characteristics are : - Viscosity index (ISO 1628-2):112 ml/g,(K value:67). Apparent density (ISO 60 ):0.60 g/ml.
- rapid fusion giving improved mechanical properties.
* RECOMMENDED APPLICATIONS - All types of rigid pipes, particularly for water supply pipes.