Arkema Lacovyl® PB 1202 PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinyl Chloride; Polyvinylchloride
Material Notes: LACOVYL PB 1202 is a vinyl homopolymer manufactured by microsuspension polymerization process for the preparation of plastisols in particular for chemical foams with low plasticizer content. * MAIN CHARACTERISTICS - Viscosity index (ISO 1628-2):110 ml/g,(K value:67).
* APPLICATIONS LACOVYL PB 1202 is recommended for the following applications: - crystal, high gloss surface coats,
- low weight coatings, pigmented, compact or cellular for wall covering,
- foam layer for flooring and coated fabrics,
- rotary screen printing,
- highly filled back coats (200 phr),
- cap closures.
ISO data provided by the manufacturer, Arkema.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|