Arkema Lacovyl® PB 8050 PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinyl Chloride; Polyvinylchloride
Material Notes: LACOVYL PB 8050 is a vinyl chloride homopolymer obtained by the mass polymerization process. It can be incorporated with plastisol based on microsuspension - or emulsion - polymerized PVC to : - obtain a lower-cost formulation,
- reduce and stabilize viscosity in storage,
- enhance pseudo-plasticity,
- reduce gloss in surface layers,
- improve transparency and thermal stability.
By virtue of its exceptionally fine state of division, it can be used in the thinnest possible layers. It is usable in every type of application, at up to 50 phr in certain cases. * MAIN PROPERTIES - Viscosity index (ISO 1628-2):79 ml/g,(K value:57).
* APPLICATIONS LACOVYL PB 8050 can be used in all plastisol applications in the manufacture of materials for - the building industry (floor and wall coverings),
- the motor industry (artificial leather and mastics),
- the food industry (closures, etc...),
- morocco-leather goods, footwear (artificial leather), etc.
- toys, balls, dolls, etc.
ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Viscosity Test
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|