Arkema Lacovyl® S 071 S PVC

 

Subcategory: Vinyl; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: Polyvinyl Chloride; Polyvinylchloride

Material Notes:
LACOVYL S 071 S is a low molecular weight vinyl chloride homopolymer produced by a suspension polymerization process.

Characteristics :

_ Viscosity index (ISO 1628-2):79 ml/g,(K value:57). Apparent density (ISO 60):0.58 g/ml.

  • good low temperature fusion characteristics.
  • suitable for dry blend preparation providing a controlled feed to production machines.
  • excellent base color and thermal stability.

Provides finished products with good transparency and free from fish eyes.

* RECOMMENDED APPLICATIONS

  • Bottles by extrusion and injection blow molding. LACOVYL is also recommended for biaxial orientation processes.
  • Calendering of rigid sheet.
  • Extrusion of rigid film and sheet.

* EXAMPLES OF APPLICATIONS

PVC-U:

  • NAKAN RMA 705 N
  • NAKAN RMS 501 L

ISO data provided by the manufacturer, Arkema.

Available Properties
  • Viscosity Test
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。