Arkema Lacovyl® S 071 S PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinyl Chloride; Polyvinylchloride
Material Notes: LACOVYL S 071 S is a low molecular weight vinyl chloride homopolymer produced by a suspension polymerization process. Characteristics : _ Viscosity index (ISO 1628-2):79 ml/g,(K value:57). Apparent density (ISO 60):0.58 g/ml. - good low temperature fusion characteristics.
- suitable for dry blend preparation providing a controlled feed to production machines.
- excellent base color and thermal stability.
Provides finished products with good transparency and free from fish eyes. * RECOMMENDED APPLICATIONS - Bottles by extrusion and injection blow molding. LACOVYL is also recommended for biaxial orientation processes.
- Calendering of rigid sheet.
- Extrusion of rigid film and sheet.
* EXAMPLES OF APPLICATIONS PVC-U: - NAKAN RMA 705 N
- NAKAN RMS 501 L
ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Viscosity Test
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|