Arkema Lacovyl® SK 70 PVC
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinyl Chloride; Polyvinylchloride
Material Notes: LACOVYL SK 70 is a vinyl chloride homopolymer produced by a suspension polymerization process. Characteristics: - Viscosity index (ISO 1628-2):126 ml/g,(K value:71). Apparent density (ISO 60):0.48 g/ml.
- high rate of plasticizer absorption.
- high molecular weight giving articles with good mechanical properties.
- good dielectric properties.
- excellent thermal stability.
Provides finished products with good transparency and free from fish eyes. * RECOMMENDED APPLICATIONS - Sheathing and insulation of cables.
- Calendering and extrusion blow-molding of plasticized film and sheet.
- Extrusion of plasticized tube and profile.
* EXAMPLES OF APPLICATIONS PVC-P: - NAKAN FEM 781 N - NAKAN FMM 871 N - NAKAN FKJ 905 R
- NAKAN FEM 691 N - NAKAN FMM 611 N - NAKAN FSS 703 R
- NAKAN FKC 911 S - NAKAN FMS 601 L - NAKAN FKS 810 R
- NAKAN FKH 911 R - NAKAN FMS 801 L - NAKAN FSS 601 R
- NAKAN FKS 902 R - NAKAN FKS 918 R - NAKAN FKS 911 S
ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Viscosity Test
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|