Arkema Lacqrene® 8350 Polystyrene, High Impact
Subcategory: Polystyrene; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PS
Material Notes: Very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is recommended for the production of packaging intended for products likely to cause stress cracking e.g. fats and oils. LACQRENE 8350 retains good mechanical properties at low temperatures making this grade suitable for frozen food packaging and for the production of fridge liners in contact with HCFC expanded foam insulation. Applications: Extrusion; Sheets for thermoforming, fridge doors and cabinet liners, packaging for fatty foods. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Surface Resistance
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|