Arkema Lucalor® RB 1167 CPVC, Pipe Grade
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Chlorinated Polyvinyl Chloride
Material Notes: LUCALOR RB 1167 is the trade name for chlorinated polyvinyl (CPVC) made by Elf Atochem. It is produced with a patented mass PVC resin chlorination process. MAIN CHARACTERISTICS - Chlorine content:67.3%. Viscosity index (ISO 1628-2):94 ml/g
APPLICATIONS LUCALOR RB 1167 is particularly designed for production of pipes that have to withstand heat and pressure. It is used in the building industry for: - Central heating pipes
- Pipes for hot water distribution for domestic purposes and in the chemical industry,
- Pipes carrying for fluids under pressure.
EXAMPLES OF APPLICATIONS Compounds of CPVC: - LUCALOR PEY 221
- LUCALOR PEY 333
- LUCALOR PEY 436.
ISO data provided by the manufacturer, Arkema.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|