Arkema Nakan® RMA 705 N PVC, Rigid Injection Molding Grade
Subcategory: Vinyl; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyvinyl Chloride; Polyvinylchloride
Material Notes: NAKAN RMA 705 N L is a rigid polyvinyl chloride compound developed for injection molding of various medium impact resistance applications. ISO data provided by the manufacturer, Arkema.