Arkema Orgalloy® LE 6000IH Nylon Alloy, Flexible Grade (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon, Other
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Polyamide
Material Notes: LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents). medium viscosity and stiffness, specially suited to the covering of cable and tube. Also suited to injection molding. Flame retardant grade. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Comparative Tracking Index
- Melting Point
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|