Arkema Orgalloy® RS 6635 A Nylon 66 Alloy, 35% Glass Fiber (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA66; Polyamide 66, Nylon 6,6; Polyamide 6,6
Material Notes: RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties. For injection molding. 35% glass fiber, with improved hydrolysis and thermal resistance. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|