Arkema Oroglas® HFI-10 Acrylic, Impact Grade
Subcategory: Acrylic; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Material Notes: OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time. Key features :
- impact resistance: up to 10 times more impact-resistant than standard acrylic
- easy processing: flow significantly improved which contribute to reduce cycle time by 20 %.
( MFI, 230°c/3.8 kg ) = 3 gr / 10 min ( MVI, 230°c/3.8 kg ) = 2.8 ml / 10 min - excellent optical properties with low edge color
- UV stability
Typical applications : OROGLAS HFI-10 can be injection molded or extruded in any type of machine Typical applications are in the fields of: building, lighting, appliances, information technology, and business machines. OROGLAS HFI-10 is recommended when toughness and increased flow are required. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|