Arkema Oroglas® MI-7T Acrylic
Subcategory: Acrylic; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Material Notes: OROGLAS MI-7T is a medium impact grade combining excellent thermal resistance with good impact performance. Key features : - impact resistance: up to 7 times more impact-resistant than standard acrylic
- high temperature resistance: HDT A / 1.82 MPa = 93°c
- excellent optical properties
- UV stability
- brilliance and scratch resistance
- low edge color
- easy processing
Typical applications : OROGLAS MI-7T can be injection or extruded for several types of applications in the following fields: automotive, appliances, business machines building, etc... ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|