Arkema Oroglas® SG 10 Acrylic, Gamma Radiation Resistant
Subcategory: Acrylic; Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Material Notes: OROGLAS SG 10 is special Gamma - radiation - resistant formulation designed for use in medical devises. OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse effect on physical properties. In addition, OROGLAS SG 10 has all the features of oroglas high impact grades including increased flow, clarity and chemical resistance. OROGLAS SG 10 meets FDA and pharmacopeia XXI class VI toxicity requirements. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|