Arkema Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Dry)
Subcategory: Elastomer, TPE; Polyether Block Amide (PEBA); Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Thermoplastic Elastomer, TPE
Material Notes: POLYETHER BLOCK AMIDE (PEBA) hardness 72 shore D Highest modulus PEBAX Applications: medical, extrusion Sport ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Hardness, Shore D
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Melting Point
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|