Arkema Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned)
Subcategory: Elastomer, TPE; Polyether Block Amide (PEBA); Thermoplastic
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: Thermoplastic Elastomer, TPE
Material Notes: POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable... ISO data provided by the manufacturer, Arkema.