Arkema Rilsan® Powder T Blue X 7421 AC Nylon 11, Coating Grade
Subcategory: Nylon; Thermoplastic; Nylon 11
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Powder T BLUE X 7421 AC - RILSAN POLYAMIDE 11 (PA11) POWDER Blue Powder pigmented by Dry Blend, designed for the coating of tubes, pipe systems, flanges and fittings for the transport of fluids in particular potable water. Coating done by dipping of pre heated part in a bed of fluidized powder. Submitted to potable water approval. The range includes several colors. The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Melting Point
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|