Arkema Rilsan® Powder T White 7050 Nylon 11, Coating Grade
Subcategory: Nylon; Thermoplastic; Nylon 11
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Powder T WHITE 7050 - RILSAN POLYAMIDE 11 (PA11) POWDER White powder specially developed for coating of dishwasher baskets. Approved for food contact. Can be applied by dipping the pre heated basket in a bed of fluidized powder. The range includes several colors. The properties listed in the data base have been measured on a corresponding RILSAN PA11 Granule. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Melting Point
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|