Arkema Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 11
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Designation ISO 1874-PA11/xx,E,18-002 Transparent and flexible copolymer for tubes extrusion. Additive free. High flexibility. Very good transparency. High chemical resistance. USP XXIII class VI approval. Example applications: Catheters. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|