Arkema Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Dry)
Subcategory: Nylon; Thermoplastic; Nylon 12
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12-P,EHL,22-005 Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant. Flexibility. Very good ability to overmold Pebax and Rilsan. Easy to color. Example applications: Sport footwear soles. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Melting Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|