Arkema Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Dry)
Subcategory: Nylon; Thermoplastic; Nylon 12
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12-P,MHLR,14-004 Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent. Good impact strength. Flexibility and dynamic properties even at low temperatures. Easy filling of the mold due to its well adapted viscosity. Low shrinkage: include 1% on average for the design of the mold. Good dimensional stability (low moisture absorption). Example applications: Flexible parts with high impact strength and vibration resistance. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Melting Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|