Arkema Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,M,16-090,CF20 Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Antistatic properties. Example applications: Parts with high mechanical properties and dimensional precision. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|