Arkema Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-020,GB30 Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent. Reinforced isotropic performances. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption). Low coefficient of linear expansion. Example applications: Mechanical parts with dimensional precision. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|