Arkema Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-030,GF15 Rigid grade with glass fiber filler (15%) for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent. Rigidity combined with good impact strength. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. Example applications: Mechanical fittings. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|