Arkema Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Dry)
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA12; Polyamide 12
Material Notes: Designation ISO 1874-PA12,MHLR,16-050,GF30 Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent. High rigidity. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability. UL classification: UL94 HB (3,05mm) RTI(C) 65/65/65 Example applications: Mechanical parts with high rigidity. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Melting Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|