Arkema Rilsan® BESN P20 TL Nylon 11, Flexible Tubing Grade (Dry)
Subcategory: Nylon; Thermoplastic; Nylon 11
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Designation ISO 1874-PA11-P,EHL,22-004 Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized. Flexibility. High impact strength. Very good chemical resistance. Ability to be processed at high speed. Example applications: Flexible tubes for automotive. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Melting Point
- Flammability, UL94
|
|
|
|