Arkema Rilsan® BMN Y TLD Nylon 11, MoS2 Filled (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 11; Polymer
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Designation ISO 1874-PA11,MHLR,12-020,MD05 Rigid grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold release agent. No need of lubricant. Low friction coefficient. Abrasion resistance. Outstanding mechanical properties. Easy filling of the mold due to its well adapted melt viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption). UL classification: UL94 V2 (3,05mm) RTI(C) 105/90/105 Example applications: Moving mechanical parts with friction such as gear or bearing. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|