Arkema Rilsan® KMVO 39099 TL Nylon 11 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 11
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Designation ISO 1874-PA11,MHL,18-010 Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized. Low shrinkage: include 1% on average for the design of the mold. High dimensional stability due to its low moisture absorption. Potable water contact approval WRC 940 7502. Example applications: All sort of pieces for food applications. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|