Arkema Rilsan® MB 3501 Nylon 11, Flexible Tubing Grade (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 11
Close Analogs: Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.
Key Words: PA11; Polyamide 11
Material Notes: Designation ISO 1874-PA11-HI,MHL,22-004 Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized. Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Good chemical resistance. Example applications: Tubes for air brake system. approved by ISO 7628, DIN 73378 (PA11-PHLY), NFR 12632, SAEJ 844. ISO data provided by the manufacturer, Arkema.
| Available Properties |
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|