AT Plastics Ateva® 1062 Ethylene Vinyl Acetate Copolymer Film
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Close Analogs: This grade is not listed with the AT Plastics standard product line.
Material Notes: Laminating and coextrusion; excellent sealability, opticals, strength, and antiblocking characteristics. Information provided by AT Plastics.
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Dart Drop Test
- Melting Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|