AT Plastics Ateva® 1821 Ethylene Vinyl Acetate Copolymer Compounding Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Close Analogs: This grade is not listed with the AT Plastics standard product line.
Material Notes: Well suited for compound and masterbatch applications. Information provided by AT Plastics.
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Yield Strength
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|