AT Plastics Ateva® 1806A Ethylene Vinyl Acetate Copolymer
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: hot melt coatings and in sound deadening/mass back applications
Material Notes: Ateva® 1806A resin is suitable for use in hot melt coatings, and in sound deadening/mass back applications. It contains an antioxidant to minimize viscosity changes of the hot melt blends during processing. It complies with Code of Federal Regulation 21 CFR Section 177.1350 and 175.105, subject to extraction limitations for specific end use applications. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives: AntioxidantApplications: Adhesives & Sealants; Automotive
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Ring & Ball Softening Point
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|