AT Plastics Ateva® 2861AU Ethylene Vinyl Acetate Copolymer
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: low temperature sealing superior bonds and UV protection
Material Notes: Ateva® 2861AU resin is well suited for extrusion coating and co-extrusion applications where low temperature sealing superior bonds and UV protection are required. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives: UV Blocker AntioxidantApplications: Extrusion Coating & Laminating
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Melting Point
- Vicat Softening Point
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|