AT Plastics AT 418 Low Density Polyethylene (LDPE)
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: extrusion coating and lamination applications as well as blending, injection molding, and profile extrusion
Material Notes: AT 418 resin is well suited for extrusion coating and lamination applications as well as blending, injection molding, and profile extrusion applications. This resin has excellent adhesion and low neck-in at high speeds. This polymer may be processed on conventional extrusion equipment. A melt temperature in the 280-320°C range is recommended for this resin.Applications: Extrusion Coating & Laminating; Molding & Miscellaneous
| Available Properties |
- Density
- Thickness
- Melt Flow
- Coating Weight
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Line Speed ft/min
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|