AT Plastics Ateva® 1062ASB Ethylene Vinyl Acetate Copolymer Film
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: co-extrusion applications with excellent sealabilty, strength, and low COF
Material Notes: Ateva® 1062ASB resin is suitable for co-extrusion applications with excellent sealabilty, strength, and low COF. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. Properties listed are for a film produced on a three layer co-extrusion with a 76 mm die, at a stock temperature of 210°C. Additives: Slip / AntiblockApplications: Flexible Packaging
| Available Properties |
- Density
- Vinyl Acetate Content
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Dart Drop
- Melting Point
- Haze
- Gloss
- Blow-up Ratio (BUR)
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|