AT Plastics Ateva® 1081 Ethylene Vinyl Acetate Copolymer Film
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer; Film
Key Words: film extrusion requiring superior sealability and strength
Material Notes: Ateva® 1081 resin is well suited for film extrusion requiring superior sealability and strength. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Properties listed are for a film produced on a 24:1 L/D, 40 mm extruder with a 100 mm die, at a melting temperature of 210°C. Additives: Applications: Flexible Packaging
| Available Properties |
- Density
- Vinyl Acetate Content
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Dart Drop
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
- Blow-up Ratio (BUR)
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|