AT Plastics Ateva® 1081 Ethylene Vinyl Acetate Copolymer
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Key Words: medical tubing
Material Notes: Ateva® 1081 resin is designed for medical tubing, it is also recommended for tubing applications. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Additives: Applications: Medical; Tubes & Pipes
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|